Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastron V100.A78.B - TPV - Elastron Kimya A.S.

Material Data Center offers the following functions for Elastron V100.A78.B:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Elastron V datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Технологические и физические свойстваЗначениеЕдиницаСтандарт
Данные ASTM
Усадка при литье, продольная 0.0201 мм/мм ASTM D 955
Усадка при литье, поперечная 0.014 мм/мм ASTM D 955
Механические свойстваЗначениеЕдиницаСтандарт
Данные ASTM
Предел прочности 6.5 МПа ASTM D 638
Относительное удлинение при разрыве 450 % ASTM D 638
Модуль при 100% удлинении 2.4 МПа ASTM D 412
Модуль при 300% удлинении 4.5 МПа ASTM D 412
Твердость по Шору А 78 - ASTM D 2240
Стойкость к разрыву 38 кН/м ASTM D 624
Остаточная деформация при сжатии, 22 чч @ 73 °F/ 22,8°C 26 % ASTM D 395
Остаточная деформация при сжатии, 22 чч @ 158 °F/ 70°C 38 % ASTM D 395
Теплофизические свойстваЗначениеЕдиницаСтандарт
Данные ASTM
Класс огнестойкости (категория горючести) по стандарту UL 94 (ПВ-0) HB - UL 94
Прочие свойстваЗначениеЕдиницаСтандарт
Плотность 930 кг/м³ ASTM D 792
Особые свойства и характеристики
Способы переработки
Литье под давлением
Вид поставки
Черный
Специальные характеристики
Мягкий на ощупь
Химическая стойкость
Стойкость к действию озона
Доступность материала по регионам
Европа
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.